If levelling needs to be improved Ultramax 30 can be added in increments of 0.5 ml/litre of plating solution. An overdose of Ultramax 30 may cause low current density dullness. This can easily be rectified by plating out at low current density.

Overview

Ultramax 30 leveller maintains the high-speed levelling properties of the nickel-plating solution.